X80管线钢焊接接头的模拟重构及电偶腐蚀行为表征
|
|
Reconstruction and Characterization of Galvanic Corrosion Behavior of X80 Pipeline Steel Welded Joints
|
|
图5. EIS的等效电路模型 |
Fig.5. Equivalent circuit for fitting EIS data (Rs—solution resistance, CPEf—capacitance of corrosion scale, Rpore—resistance of defects, Cdl—double layer capacitance, Rp—polarization resistance, RL—inductive resistance, L—inductance) |
![]() |