		X80管线钢焊接接头的模拟重构及电偶腐蚀行为表征
		 | 
| 
			Reconstruction and Characterization of Galvanic Corrosion Behavior of X80 Pipeline Steel Welded Joints
			 | 
| 图2. X80钢焊接接头各部分的显微组织 | 
| Fig.2. Microstructures of X80 steel (AF—acicular ferrite, MF—massive ferrite, QF—quasi-polygonal ferrite, M-A— | 
|  |