退火温度对TWIP钢组织性能和氢致脆性的影响
|
|
Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel
|
|
图3. Fe-18Mn-0.6C TWIP钢退火板未充氢条件下拉伸得到的工程应力-应变曲线 |
Fig.3. Engineering stress-engineering strain curves of Fe-18Mn-0.6C TWIP steel annealed sheets without hydrogen charging |
![]() |