退火温度对TWIP钢组织性能和氢致脆性的影响
|
|
Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel
|
|
图4. Fe-18Mn-0.6C TWIP钢退火板未充氢条件下拉伸得到的应变硬化速率和加工硬化指数随真应变的变化关系曲线 |
Fig.4. Curves of strain hardening rate (a) and strain hardening exponent (n) (b) vs true strain of Fe-18Mn-0.6C TWIP steel annealed sheets without hydrogen charging |
![]() |