[an error occurred while processing this directive]
316L奥氏体不锈钢非对称载荷下的疲劳与循环塑性行为
彭剑1,2(),高毅1,代巧2,3,王颖1,李凯尚1
Fatigue and Cycle Plastic Behavior of 316L Austenitic Stainless Steel Under Asymmetric Load
Jian PENG1,2(),Yi GAO1,Qiao DAI2,3,Ying WANG1,Kaishang LI1

图3. 316L奥氏体不锈钢在不同循环载荷作用下平均应变的演化规律

Fig.3. Evolutions of mean strain with cyclic number at different cycle loads of 316L austenitic stainless steel (Inset shows the mean strain evolution above 570 MPa)