高强耐蚀管钢点状偏析及带状缺陷的特征与演变
李博1,张忠铧2,刘华松1,罗明2,兰鹏1,唐海燕1,张家泉1()
Characteristics and Evolution of the Spot Segregations and Banded Defects in High Strength Corrosion Resistant Tube Steel
Bo LI1,Zhonghua ZHANG2,Huasong LIU1,Ming LUO2,Peng LAN1,Haiyan TANG1,Jiaquan ZHANG1()

图6. 铸坯点状偏析区域枝晶形貌与EPMA面扫描和线扫描分析结果

Fig.6. Dendritic morphology and EPMA analyses of map scanning (a) and line scanning (b) in the spot segregation zones