[an error occurred while processing this directive]
Fe-Cu-Pb合金液-液相分离及废旧电路板混合金属分级分离与回收
陈斌1,2,何杰1,2(),孙小钧1,2,赵九洲1,2,江鸿翔1,张丽丽1,郝红日1
Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards
Bin CHEN1,2,Jie HE1,2(),Xiaojun SUN1,2,Jiuzhou ZHAO1,2,Hongxiang JIANG1,Lili ZHANG1,Hongri HAO1

图9. 不同转速下1473 K时富Fe液滴以及1233 K时富Pb液滴在Cu基体的运动速率(νS、ν'S)与液滴半径的关系

Fig.9. The motion rates (νS, ν'S) of the Fe-rich droplets at 1473 K and the Pb-rich droplets in Cu matrix at 1233 K at different rotation rates