Fe-Cu-Pb合金液-液相分离及废旧电路板混合金属分级分离与回收
陈斌1,2,何杰1,2(),孙小钧1,2,赵九洲1,2,江鸿翔1,张丽丽1,郝红日1
Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards
Bin CHEN1,2,Jie HE1,2(),Xiaojun SUN1,2,Jiuzhou ZHAO1,2,Hongxiang JIANG1,Lili ZHANG1,Hongri HAO1

图7. 超重力场中,MFeC-MPCB-MPb-MAl (质量比MFeC∶MPCB∶MPb∶MA=0.8∶1∶1.1∶0.1)、MFeC-MPCB (质量比MFeC∶MPCB=0.8∶1)和MCu-rich zone-MPb-MAl (质量比MCu-rich zone∶MPb∶MAl=1∶1.1∶0.1)铸锭切面的OM像(n=4500 r/min),及离心分离得到的Cu枝晶与富Pb物质

Fig.7. OM images of the sections of MFeC-MPCB-MPb-MAl (mass ratio MFeC∶MPCB∶MPb∶MAl=0.8∶1∶1.1∶0.1) (a), MFeC-MPCB (mass ratio MFeC∶MPCB=0.8∶1) (b), MCu-rich zone-MPb-MAl (mass ratio MCu-rich zone∶MPb∶MAl=1∶1.1∶0.1) (c) ingots solidified in super-gravity field (rotation rate n=4500 r/min); and Cu dendrites (d) and Pb-rich substance (e) obtained by centrifugal separation