Fe-Cu-Pb合金液-液相分离及废旧电路板混合金属分级分离与回收
陈斌1,2,何杰1,2(),孙小钧1,2,赵九洲1,2,江鸿翔1,张丽丽1,郝红日1
Liquid-Liquid Phase Separation of Fe-Cu-Pb Alloy and Its Application in Metal Separation and Recycling of Waste Printed Circuit Boards
Bin CHEN1,2,Jie HE1,2(),Xiaojun SUN1,2,Jiuzhou ZHAO1,2,Hongxiang JIANG1,Lili ZHANG1,Hongri HAO1

图5. 三元(Fe0.4Cu0.6)72Pb28合金凝固过程示意图

Fig.5. Schematics of solidification process of ternary (Fe0.4Cu0.6)72Pb28 alloy (a~e)