Ti2AlNb异形粉末环件的轧制成形与性能研究
|
|
Ring Rolling Forming and Properties of Ti2AlNb Special Shaped Ring Prepared by Powder Metallurgy
|
|
图1. Ti2AlNb预合金粉末的独立粒度分布 |
Fig.1. Differential size distribution of Ti2AlNb pre-alloyed powder |
![]() |