Ti2AlNb异形粉末环件的轧制成形与性能研究
|
|
Ring Rolling Forming and Properties of Ti2AlNb Special Shaped Ring Prepared by Powder Metallurgy
|
|
图 12. Ti2AlNb异形粉末环坯轧制前后显微组织的SEM像 |
Fig.12. Low (a, c) and high (b, d) magnified SEM images of Ti2AlNb PM alloy |
![]() |