Ti2AlNb异形粉末环件的轧制成形与性能研究
|
|
Ring Rolling Forming and Properties of Ti2AlNb Special Shaped Ring Prepared by Powder Metallurgy
|
|
图 10. Ti2AlNb合金的应变速率敏感因子(m)比较 |
Fig.10. Counter maps of strain rate sensitivity value (m) for HIP (a) and wrought (b) Ti2AlNb alloys |
![]() |