B含量对K417G合金凝固过程中组织演变和力学性能的影响
|
|
Effect of Boron Content on Microstructure Evolution During Solidification and Mechanical Properties of K417G Alloy
|
|
图8. 不同B含量K417G合金900 ℃、315 MPa持久性能 |
Fig.8. Stress rupture properties at 900 ℃ and 315 MPa of K417G alloy with different B contents |
![]() |