变形参数对2195 Al-Li合金动态再结晶的影响
李旭1,杨庆波1,樊祥泽1,呙永林2,林林2,张志清1,3()
Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy
Xu LI1,Qingbo YANG1,Xiangze FAN1,Yonglin GUO2,Lin LIN2,Zhiqing ZHANG1,3()

图5. 2195 Al-Li合金变形组织的EBSD像

Fig.5. Electron backscatter diffraction (EBSD) images of 2195 Al-Li alloy deformed at different lnZ (CDRX—continuous dynamic recrystallization, GDRX—geometric dynamic recrystallization, DDRX—discontinuous dynamic recrystallization)