变形参数对2195 Al-Li合金动态再结晶的影响
李旭1,杨庆波1,樊祥泽1,呙永林2,林林2,张志清1,3()
Influence of Deformation Parameters on Dynamic Recrystallization of 2195 Al-Li Alloy
Xu LI1,Qingbo YANG1,Xiangze FAN1,Yonglin GUO2,Lin LIN2,Zhiqing ZHANG1,3()

图1. 试样分析位置

Fig.1. Schematic of observing areas (RD, TD, ND represent rolling, transverse and normal directions, respectively; EBSD—electron backscatter diffraction; TEM—transmission electron microscope)