冷轧态Ti-35Nb-2Zr-0.3O合金的异常热膨胀行为
蓝春波1,2,梁家能1,劳远侠1,谭登峰1,黄春艳1,莫羡忠1,庞锦英1()
Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy
Chunbo LAN1,2,Jianeng LIANG1,Yuanxia LAO1,Dengfeng TAN1,Chunyan HUANG1,Xianzhong MO1,Jinying PANG1()

图3. Ti-35Nb-2Zr-0.3O合金在固溶态及不同形变下的XRD谱

Fig.3. XRD spectra of Ti-35Nb-2Zr-0.3O alloy under ST and different CR deformation reductions