冷轧态Ti-35Nb-2Zr-0.3O合金的异常热膨胀行为
蓝春波1,2,梁家能1,劳远侠1,谭登峰1,黄春艳1,莫羡忠1,庞锦英1()
Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy
Chunbo LAN1,2,Jianeng LIANG1,Yuanxia LAO1,Dengfeng TAN1,Chunyan HUANG1,Xianzhong MO1,Jinying PANG1()

图6. 90%形变Ti-35Nb-2Zr-0.3O合金在室温至850 ℃的热膨胀曲线和膨胀系数曲线

Fig.6. Thermal expansion and expansion coefficient curves of 90%CR Ti-35Nb-2Zr-0.3O alloy from room temperature to 850 ℃