冷轧态Ti-35Nb-2Zr-0.3O合金的异常热膨胀行为
|
蓝春波 1,2,梁家能 1,劳远侠 1,谭登峰 1,黄春艳 1,莫羡忠 1,庞锦英 1( )
|
Anomalous Thermal Expansion Behavior of Cold-RolledTi-35Nb-2Zr-0.3O Alloy
|
Chunbo LAN 1,2,Jianeng LIANG 1,Yuanxia LAO 1,Dengfeng TAN 1,Chunyan HUANG 1,Xianzhong MO 1,Jinying PANG 1( )
|
|
图1. Ti-35Nb-2Zr-0.3O合金固溶态及不同形变的OM像
|
Fig.1. OM images of Ti-35Nb-2Zr-0.3O alloy under ST (a), 30%CR (b), 60%CR (c) and 90%CR (d) (ST—solution treated, CR—cold rolled, RD—rolling direction. Arrows in Figs.1b and c show the deformation bands) |
|
|
|
|