[an error occurred while processing this directive]
电子束快速成形制备TC4合金的组织和拉伸性能分析
刘征1,2,刘建荣1(),赵子博1,王磊1,王清江1,杨锐1
Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing
Zheng LIU1,2,Jianrong LIU1(),Zibo ZHAO1,Lei WANG1,Qingjiang WANG1,Rui YANG1

图3. 原始β晶粒和α板条宽度与沉积高度的关系

Fig.3. The changes of the prior β grain size and the width of α lath along the building height