电子束快速成形制备TC4合金的组织和拉伸性能分析
刘征1,2,刘建荣1(),赵子博1,王磊1,王清江1,杨锐1
Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing
Zheng LIU1,2,Jianrong LIU1(),Zibo ZHAO1,Lei WANG1,Qingjiang WANG1,Rui YANG1

图7. 拉伸试样的对数真应力-对数真应变曲线(应变2.5%~4.6%)和加工硬化指数

Fig.7. True stress-true stain curves plotted on logarithmic axes in plastic portion between 2.5% and 4.6% strain for the tensile samples at different Z direction height and work hardening exponent (σ—true stress, ε—true strain, n—work hardening exponent)