电子束快速成形制备TC4合金的组织和拉伸性能分析
刘征1,2,刘建荣1(),赵子博1,王磊1,王清江1,杨锐1
Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing
Zheng LIU1,2,Jianrong LIU1(),Zibo ZHAO1,Lei WANG1,Qingjiang WANG1,Rui YANG1

图5. TC4合金α相的{0001}和{101ˉ0}极图

Fig.5. Pole figures of {0001} (a) and {101ˉ0} (b) for the α phase in the TC4 alloy