电子束快速成形制备TC4合金的组织和拉伸性能分析
|
|
Microstructure and Tensile Property of TC4 Alloy Produced via Electron Beam Rapid Manufacturing
|
|
图1. 电子束快速成形(EBRM)制备TC4合金的示意图和拉伸试样的取样位置示意图 |
Fig.1. Schematics of the TC4 alloy produced by electron beam rapid manufacturing (EBRM) (a) and sampling location of tensile specimens (b) (X direction is the electron beam scanning direction, Z direction is the building direction) |
![]() |