定向凝固糊状区枝晶粗化和二次臂迁移的实验和模拟 |
|||||||||||||||||||||||||||
| 方辉,薛桦,汤倩玉,张庆宇,潘诗琰,朱鸣芳 | |||||||||||||||||||||||||||
|
Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification: |
|||||||||||||||||||||||||||
| Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU | |||||||||||||||||||||||||||
| 表2 SCN-2.0%ACE合金在不同温度梯度条件下枝晶臂迁移速率的实验值和解析解比较 | |||||||||||||||||||||||||||
| Table 2 Comparisons of experimental data and analytical predictions regarding the average migrating velocity within 18 s as a function of temperature gradient for a SCN-2.0%ACE alloy at Vp=0 μm/s and initial position y0=5037 μm (Dimensionless initial position |
|||||||||||||||||||||||||||
|
|||||||||||||||||||||||||||