定向凝固糊状区枝晶粗化和二次臂迁移的实验和模拟
方辉,薛桦,汤倩玉,张庆宇,潘诗琰,朱鸣芳

Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:
Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU
表1 本工作采用的物性参数[23,34]
Table 1 The physical parameters used in the present work[23,34]
ParameterUnitValue
Gibbs-Thomson coefficient, Γ℃·m6.48×10-8
Diffusion coefficient in liquid, Dlm2·s-11×10-9
Diffusion coefficient in solid, Dsm2·s-11×10-12
Partition coefficient, k-0.1
Liquidus slope, ml℃·%-1 (mass fraction)-2.8
Melting point of the pure solvent, Tm℃58.081