定向凝固糊状区枝晶粗化和二次臂迁移的实验和模拟
方辉1,薛桦1,汤倩玉1,张庆宇1,潘诗琰2,朱鸣芳1()
Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:
Hui FANG1,Hua XUE1,Qianyu TANG1,Qingyu ZHANG1,Shiyan PAN2,Mingfang ZHU1()

图1. 透明材料定向凝固原位观察实验装置示意图

Fig.1. Schematic of in situ experimental observation setup for directional solidification of transparent materials