触变注射成形法制备石墨烯纳米片增强镁基复合材料
张婷,赵宇宏(),陈利文,梁建权,李沐奚,侯华
Graphene Nanoplatelets Reinforced Magnesium Matrix Composites Fabricated by Thixomolding
Ting ZHANG,Yuhong ZHAO(),Liwen CHEN,Jianquan LIANG,Muxi LI,Hua HOU

图10. 触变注射成形后AZ91D镁合金及GNPs/AZ91D复合材料的拉伸曲线

Fig.10. Tensile curves of AZ91D and GNPs/AZ91D composites fabricated by thixmolding