[an error occurred while processing this directive]
触变注射成形法制备石墨烯纳米片增强镁基复合材料
张婷,赵宇宏(),陈利文,梁建权,李沐奚,侯华
Graphene Nanoplatelets Reinforced Magnesium Matrix Composites Fabricated by Thixomolding
Ting ZHANG,Yuhong ZHAO(),Liwen CHEN,Jianquan LIANG,Muxi LI,Hua HOU

图8. 触变注射成形后0.6%GNPs/AZ91D复合材料的TEM和HRTEM像

Fig.8. TEM (a) and HRTEM (b) images of 0.6%GNPs/AZ91D composite fabricated by thixmolding