[an error occurred while processing this directive]
Ag/Ti2AlC复合材料的电弧侵蚀及退化机理
丁健翔1,2,田无边2,汪丹丹2,张培根2,陈坚2,孙正明2()
Arc Erosion and Degradation Mechanism ofAg/Ti2AlC Composite
Jianxiang DING1,2,Wubian TIAN2,Dandan WANG2,Peigen ZHANG2,Jian CHEN2,Zhengming SUN2()

图6. 放电1次后Ag/10TAC触头表面过渡区域微结构、元素组成和元素面分布

Fig.6. Microstructures and element compositions of transition regions A (a) and B (b) on the Ag/10TAC contact surface (in Fig.4a) after 1-time discharging (Inset shows the enlarged image of Ti2AlC) and EDS element map results of transition regions A (c) and B (d)