Ag/Ti2AlC复合材料的电弧侵蚀及退化机理
丁健翔,田无边,汪丹丹,张培根,陈坚,孙正明

Arc Erosion and Degradation Mechanism ofAg/Ti2AlC Composite
Jianxiang DING,Wubian TIAN,Dandan WANG,Peigen ZHANG,Jian CHEN,Zhengming SUN
表1 图9b中黑色块体的EDS分析
Table 1 EDS analyses of dark block in Fig.9b (atomic fraction / %)
ElementPoint 1Point 2Point 3
Ag3.042.943.20
Ti28.9624.6822.75
Al8.046.565.86
C17.1023.6219.05
O42.8642.2049.14
Ti/Al3.603.763.88
O/Ti1.481.712.16