镍基单晶高温合金叶片模拟件平台处的枝晶生长和取向演化
|
|
Dendrite Growth and Orientation Evolution in the Platform of Simplified Turbine Blade for Nickel-Based Single Crystal Superalloys
|
|
图5. 平台3底面枝晶汇聚界面处的取向演化 |
Fig.5. Misorientation evolutions along CBDA within the platform base of platform 3 when the withdrawal rate is 9 mm/min (Orientations of dendrite arms located in the upside of CBDA are given in blue circles and those in the downside of CBDA are given in red circles)Color online |
![]() |