[an error occurred while processing this directive]
脉冲电流作用下TiAl合金凝固组织演变及形成机理
陈占兴,丁宏升(),陈瑞润,郭景杰,傅恒志
Microstructural Evolution and Mechanism of Solidified TiAl Alloy Applied Electric Current Pulse
Zhanxing CHEN,Hongsheng DING(),Ruirun CHEN,Jingjie GUO,Hengzhi FU

图6. 脉冲电流对Ti-48Al-2Cr-2Nb合金片层间距的影响