保护气成分对1000 MPa级高强熔敷金属组织特征的影响
安同邦1,2(),魏金山1,单际国2,田志凌1
Influence of Shielding Gas Composition on Microstructure Characteristics of 1000 MPa Grade Deposited Metals
Tongbang AN1,2(),Jinshan WEI1,Jiguo SHAN2,Zhiling TIAN1

图1. 不同保护气末层焊道熔敷金属显微组织的SEM像

Fig.1. SEM images of the as-deposited top beads with different shielding gases (Bc—coalesced bainite)(a) 95%Ar+5%CO2 (b) 90%Ar+10%CO2 (c) 80%Ar+20%CO2 (d) 70%Ar+30%CO2