热轧板退火工艺对19Cr2Mo1W铁素体不锈钢织构与成形性能的影响
刘后龙,马明玉,刘玲玲,魏亮亮,陈礼清()
Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel
Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN()

图8. 热轧板不同温度退火后的冷轧退火板的拉伸应力-应变曲线

Fig.8. Stress-strain curves of cold-rolled and annealed steels with hot band annealing at various temperatures