热轧板退火工艺对19Cr2Mo1W铁素体不锈钢织构与成形性能的影响
刘后龙,马明玉,刘玲玲,魏亮亮,陈礼清()
Effect of Hot Band Annealing Processes on Texture and Formability of 19Cr2Mo1W Ferritic Stainless Steel
Houlong LIU,Mingyu MA,Lingling LIU,Liangliang WEI,Liqing CHEN()

图5. 铁素体不锈钢热轧板不同温度退火后的晶体取向成像图

Fig.5. Orientation imaging maps of hot-rolled ferritic stainless steel bands annealed at 950 ℃ (a), 1000 ℃ (b), 1050 ℃ (c) and 1100 ℃ (d) (ND—normal direction, RD—rolling direction)Color online