[an error occurred while processing this directive]
挤压态GH3625合金冷变形过程中的组织和织构演变
高钰璧1,丁雨田1(),陈建军1,许佳玉1,马元俊1,张东2
Evolution of Microstructure and Texture During Cold Deformation of Hot-Extruded GH3625 Alloy
Yubi GAO1,Yutian DING1(),Jianjun CHEN1,Jiayu XU1,Yuanjun MA1,Dong ZHANG2

图9. 挤压态GH3625合金冷变形后的取向因子(μ)分布

Fig.9. Distribution of orientation factor (μ) after cold deformation of hot-extruded GH3625 superalloy(a) ε=35 % (b) ε=50 % (c) ε=65 %