挤压态GH3625合金冷变形过程中的组织和织构演变
高钰璧1,丁雨田1(),陈建军1,许佳玉1,马元俊1,张东2
Evolution of Microstructure and Texture During Cold Deformation of Hot-Extruded GH3625 Alloy
Yubi GAO1,Yutian DING1(),Jianjun CHEN1,Jiayu XU1,Yuanjun MA1,Dong ZHANG2

图1. 挤压态GH3625合金在冷变形过程中的微观组织及晶界特征分布演变

Fig.1. Evolution of microstructure and grain boundary characteristics distribution in cold deformation process of hot-extruded GH3625 superalloy (ε—cold reduction, LAGBs—low angle grain boundaries (green lines), HAGBs—high angle grain boundaries (black lines), TBs—twin boundaries)(a) ε=35% (b) ε=50% (c) ε=65% (d) grain boundary characteristics