电阻缝焊法制备铁基WC/金属双层涂层及其摩擦行为
王文琴1,2,王昭漫1,李玉龙1,王德3(),李淼1,陈情1
Wear Behavior of Fe-WC/Metal Double Layer Coatings Fabricated by Resistance Seam Weld Method
Wenqin WANG1,2,Zhaoman WANG1,Yulong LI1,De WANG3(),Miao LI1,Qing CHEN1

图8. 以WC为磨球时摩擦实验后2种涂层表面EDS元素分布图

Fig.8. EDS elemental mappings of worn surfaces of Coating-F (a) and Coating-C (b) against WC ball after BOD test