电阻缝焊法制备铁基WC/金属双层涂层及其摩擦行为
王文琴1,2,王昭漫1,李玉龙1,王德3(),李淼1,陈情1
Wear Behavior of Fe-WC/Metal Double Layer Coatings Fabricated by Resistance Seam Weld Method
Wenqin WANG1,2,Zhaoman WANG1,Yulong LI1,De WANG3(),Miao LI1,Qing CHEN1

图7. 以 SUS304为磨球时摩擦实验后2种涂层表面形貌

Fig.7. Worn surfaces of Coating-F (a~c) and Coating-C (d~f) against SUS304 ball after BOD test(a, d) overview of surfaces (b, e) SHA surfaces (c, f) WC surfaces