Na对于Al早期大气腐蚀的影响
陈星晨,王杰,陈德任,钟舜聪,王向峰()
Effect of Na on Early Atmospheric Corrosion of Al
Xingchen CHEN,Jie WANG,Deren CHEN,Shuncong ZHONG,Xiangfeng WANG()

图3. 纳秒激光烧蚀形貌及烧蚀孔洞深度

Fig.3. Three-dimensional topography of an ablation crater (a) and the heights of the crater (b)