Na对于Al早期大气腐蚀的影响
陈星晨,王杰,陈德任,钟舜聪,王向峰()
Effect of Na on Early Atmospheric Corrosion of Al
Xingchen CHEN,Jie WANG,Deren CHEN,Shuncong ZHONG,Xiangfeng WANG()

图1. Al大气环境腐蚀5周前后表面显微图

Fig.1. Microscopic images of Al surface before (a) and after 5 weeks (b) in atmosphere