W高压扭转显微组织演化过程TEM分析
李萍,林泉,周玉峰,薛克敏(),吴玉程
TEM Analysis of Microstructure Evolution Process of Pure Tungsten Under High Pressure Torsion
Ping LI,Quan LIN,Yufeng ZHOU,Kemin XUE(),Yucheng WU

图5. HPT变形试样累积等效应变

Fig.5.