纯W高压扭转显微组织演化过程TEM分析
|
|
TEM Analysis of Microstructure Evolution Process of Pure Tungsten Under High Pressure Torsion
|
|
图7. 纯W高压扭转不同圈数下的晶内和晶界HRTEM像 |
Fig.7. HRTEM images of tungsten grain inside and boundary processed by HPT(a~c) grain A inside, grain B inside and grain boundary under 1 turn, respectively(d~f) grain C inside, grain D inside and grain boundary under 2 turns, respectively(g~i) grain E inside, grain F inside and grain boundary under 5 turns, respectively |
![]() |