纯W高压扭转显微组织演化过程TEM分析
|
|
TEM Analysis of Microstructure Evolution Process of Pure Tungsten Under High Pressure Torsion
|
|
图2. 纯W在不同扭转圈数下HPT变形试样中晶粒与晶界显微组织的TEM像 |
Fig.2. TEM images showing the microstructures of grains (a, c, e) and grain boundaries (b, d, f) of pure tungsten processed by HPT under 1 turn (a, b), 2 turns (c, d) and 5 turns (e, f) (Insets in Figs.2a, c and e show the SAED patterns of grains) |
![]() |