奥氏体析出相激发形核的原位TEM研究
|
|
杜娟,程晓行,杨天南,陈龙庆,Mompiou Frédéric,张文征
|
In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates
|
|
Juan DU,Xiaoxing CHENG,Tiannan YANG,Longqing CHEN,Frédéric Mompiou,Wenzheng ZHANG
|
|
| 表3 原位先驱奥氏体γ1和γ4的O线解计算结果[34]及其宏观不变平面应变(P1)的相关参量 |
| |
|
| Parameter | O-line solution for γ1 | O-line solution for γ4 |
|---|
| xin | [0.32 0.52]b | [ 0.83 0.52]b | OR | (111)b~∥(011)f, 0.4° | (111)b~∥(01)f, 0.4° | | [100]b~∥[10]f, 2.3° | [00]b~∥[10]f, 1.5° | | Habit plane (p1) | ( 0.51 0.85)b | (0.07 0.85)b | | b | [100]b|[10]f | [100]b|[10]f | | D / nm | 2.2 | 2.2 | | d1 | [0.95 0.22]b | [ 0.13 0.15]b | | m1 | 1.1093 | 1.6621 |
|
|
|