奥氏体析出相激发形核的原位TEM研究
|
|
杜娟,程晓行,杨天南,陈龙庆,Mompiou Frédéric,张文征
|
In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates
|
|
Juan DU,Xiaoxing CHENG,Tiannan YANG,Longqing CHEN,Frédéric Mompiou,Wenzheng ZHANG
|
|
| 表2 激发形核奥氏体γ1~γ4的晶体学特征 |
| |
|
| Parameter | γ1 | γ2 | γ3 | γ4 |
|---|
OR | (011)b~∥(111)f 0.3° | (011)b~∥(111)f 0.2° | (01)b~∥(111)f 0.5° | (01)b~∥(111)f 0.2° | [100]b~∥[10]f 1.6° | [00]b~∥[10]f 1.6° | [100]b~∥[10]f 0.7° | [00]b~∥[10]f 1.1° | | Long axis | [0.32 0.53]b | [0.26 0.81]b | [ 0.49 0.87]b | [ 0.82 0.53]b | Habit plane | ( 0.54 0.84)b (0.41 0.54 0.73)f | - - | - - | (0.13 0.84)b (0.37 0.56 0.74)f |
|
|
|