奥氏体析出相激发形核的原位TEM研究
杜娟1,程晓行2,杨天南2,陈龙庆2,3,Mompiou Frédéric4,张文征1()
In Situ TEM Study on the Sympathetic Nucleation of Austenite Precipitates
Juan DU1,Xiaoxing CHENG2,Tiannan YANG2,Longqing CHEN2,3,Frédéric Mompiou4,Wenzheng ZHANG1()

图8. 激发形核奥氏体与先驱奥氏体周围母相的弹性相互作用能密度分布图

Fig.8. Distributions of mutual elastic strain energy density between sympathetically nucleated austenite and local stress created by pre-formed austenite