先共析渗碳体上形核的珠光体晶体学研究
|
|
徐文胜,张文征
|
An Investigation of the Crystallography of Pearlites Nucleated on the Proeutectoid Cementite
|
|
Wensheng XU,Wenzheng ZHANG
|
|
| 表3 图6中F、C、GC、WC以及A之间的晶体学位向关系 |
| Table 3 Orientation relationships between F, C, GC, WC and A in Fig.6 |
|
| Colony | F/C | F/A | C/A | F/WC or F/GC | C/WC or C/GC |
|---|
| I | Bagaryatsky[12] | Unreported | Unreported | Unreported | Discontinuous | | II | Pitsch-Petch[14,15] | Near K-S[26] | Unreported | Unreported | Near (10°) | | III | New-2[16] | Near K-S[26] | Unreported | Unreported | Discontinuous | | IV | Pitsch-Petch[14,15] | Near K-S[26] | Unreported | Bagaryatsky[12] | Discontinuous | | V | Pitsch-Petch[14,15] | Near K-S[26] | Unreported | New-3[16] | Continuous | | VI | Pitsch-Petch[14,15] | Near K-S[26] | F-E[30] | Pitsch-Petch[14,15] | Continuous |
|
|
|