[an error occurred while processing this directive]
脉冲磁场对TC4钛合金微观结构的影响及其机理探究
许擎栋1,李克俭1,蔡志鹏1,2,3(),吴瑶4
Effect of Pulsed Magnetic Field on the Microstructure of TC4 Titanium Alloy and Its Mechanism
Qingdong XU1,Kejian LI1,Zhipeng CAI1,2,3(),Yao WU4

图4. 脉冲磁场处理前后TC4试样微区KAM分布云图

Fig.4. Low (a, b) and locally high (c, d) magnified KAM distributions of the TC4 sample before (a, c) and after (b, d) pulsed magnetic treatment (The KAM distribution after treatment is more homogeneous than that before treatment totally. Positions 1, 2 and 3 in Figs.4a and b as an example indicate the variation of KAM near the grain boundaries. The boxes in Figs.4c and d forcefully indicate the reduction of KAM in the specific grain while the ellipses in Figs.4c and d indicate the increase of KAM in the specific grains. Positions 4, 5 and 6 in Figs.4c and d as an example indicate the variation of KAM and especially the variation of the shape of the grain boundaries)