冷旋锻变形对
TB9
钛合金显微组织和拉伸性能的影响
任德春
1,
2
,苏虎虎
1,
2
,张慧博
1
,王健
1
,金伟
1,
2
(
),杨锐
1,
2
Effect of Cold Rotary-Swaging Deformation on Microstructure and Tensile Properties of TB9 Titanium Alloy
Dechun REN
1,
2
,Huhu SU
1,
2
,Huibo ZHANG
1
,Jian WANG
1
,Wei JIN
1,
2
(
),Rui YANG
1,
2
图2.
TB9钛合金冷旋锻变形前后大角度晶界和小角度晶界所占比例
Fig.2.