冷旋锻变形对TB9钛合金显微组织和拉伸性能的影响
任德春1,2,苏虎虎1,2,张慧博1,王健1,金伟1,2(),杨锐1,2
Effect of Cold Rotary-Swaging Deformation on Microstructure and Tensile Properties of TB9 Titanium Alloy
Dechun REN1,2,Huhu SU1,2,Huibo ZHANG1,Jian WANG1,Wei JIN1,2(),Rui YANG1,2

图6. 冷旋锻变形量70%时的EBSD衬度对比及取向分布

Fig.6. EBSD contrast band map showing sheer bands of TB9 titanium alloy under cold rotary-swaging rate of 70% (a) and distribution of misorientation along the arrow in Fig.6a (b)